Mechanical Properties Metric English Comments
Flexural Modulus 51.7 GPa

@Temperature 22.8 °C
7500 ksi

@Temperature 73.0 °F
ASTM D790
Quadrant EPP Ketron® LSG CC PEEK Ketron PEEK with 57% Woven Carbon Fiber
Flexural Modulus 51.7 GPa
7500 ksi
Greene Tweed Xycomp® 1030-02 Carbon/Nylon 12 Composite
Greene, Tweeds Xycomp® engineered components offer a wider range of benefits than conventional thermoset resin systems because they rely on thermoplastic resins for their matrix. With specific st..