Mechanical Properties Metric English Comments
Flexural Modulus 2.06 - 3.52 GPa
299 - 511 ksi
Average value: 2.34 GPa Grade Count:37
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..