Polymer Property : Flexural Modulus = 524 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.61 GPa
524 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DX05475 PC
LNP* THERMOCOMP* DX05474 is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Flame Retardant.
Flexural Modulus 3.61 GPa
524 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF PX06416 PA 6
LNP* Thermotuf* PX06416 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Modulus 3.61 GPa
524 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOTUF PX06416 PA 6 (Asia Pacific)
LNP* Thermotuf* PX06416 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact.