Mechanical Properties Metric English Comments
Flexural Modulus 0.0700 - 36.2 GPa
10.2 - 5250 ksi
Average value: 2.51 GPa Grade Count:279
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Flexural Modulus 0.255 - 36.2 GPa
37.0 - 5250 ksi
Average value: 6.54 GPa Grade Count:334
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Flexural Modulus 0.483 - 36.2 GPa
70.0 - 5250 ksi
Average value: 4.87 GPa Grade Count:205
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Flexural Modulus 2.07 - 36.2 GPa
300 - 5250 ksi
Average value: 6.17 GPa Grade Count:106
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..