Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 38.0 GPa | 5510 ksi | |
Cytec Thornel® VCB-20 Carbon Cloth/Epoxy Composite Data provided by the manufacturer, Amoco Performance Products, Inc. Cured ply 0.47 mm thick, 55% fiber vol.Thornel® products were sold by Amoco and are now owned by Cytec. |
|||
Flexural Modulus | 38.0 GPa @Temperature 23.0 °C |
5510 ksi @Temperature 73.4 °F |
Dry; EN2562 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |