Mechanical Properties Metric English Comments
Flexural Modulus 3.834 GPa
556.1 ksi
ASTM D790
Global AS-320-PC Acrylonitrile Styrene, High Chemical/High Heat Resistance Grade
Description-transparent, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-sanitary products, electrical partsInformation provided b..