Polymer Property : Flexural Modulus = 557 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.84 GPa
557 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC
LNP* THERMOCOMP* DB008ERP is a compound based on Polycarbonate resin containing 40% Glass Bead. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 3.84 GPa
557 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC (Asia Pacific)
LNP* Thermocomp* DB008ERP is a compound based on Polycarbonate resin containing Glass Bead. Added features of this material include: Easy Molding, Mold Release.
Flexural Modulus 3.84 GPa
557 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66
LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead.
Flexural Modulus 3.84 GPa
557 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GFN1 PPE+PS
PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui..