Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.90 GPa | 565 ksi | ASTM D790 |
Multibase Multi-Pro® 3012 RC Polypropylene Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |