Polymer Property : Flexural Modulus = 597.4 ksi
Polymer Property :
Flexural Modulus =
597.4 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
4.119
GPa
597.4
ksi
ASTM D790
Kolon KOPA® KN333MT30BL Mineral Reinforced Nylon 66
MF reinforcedApplications Cam shaftsInformation provided by API-Kolon.