Mechanical Properties Metric English Comments
Flexural Modulus 6.37 GPa

@Thickness 3.20 mm
925 ksi

@Thickness 0.126 in
ASTM D790
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co..
Flexural Modulus 6.37 GPa
925 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN135HB30HI Multi Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 6.37 GPa

@Thickness 3.20 mm
925 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical Lupox® HI2303 PBT+GF30%
Description: Injection Molding, PBT+GF30%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical
Flexural Modulus 6.37 GPa
924 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant.
Flexural Modulus 6.37 GPa
924 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific)
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant.
Flexural Modulus 6.37 GPa
924 ksi
ASTM D790
SABIC Innovative Plastics NORYL FM3020V PPE+PS (Asia Pacific)
30% filled FR high modulus foam grade
Flexural Modulus 6.37 GPa
925 ksi
DIN 53452; ASTM D790
Kolon SPESIN® KP213G15 Flame Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Flexural Modulus 6.37 GPa
925 ksi
DIN 53452; ASTM D790
Kolon SPELLOY® KB133G30 PC + PBT Alloy Resin  (discontinued **)
SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional..
Flexural Modulus 6.37 GPa
925 ksi
DIN 53452; ASTM D790