Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 33% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo.. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te.. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Technetics Group Amicon™ PEEK 30% Glass Filled
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2210 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 830R PBT (Asia Pacific) 30% glass filled, release grade, polyester alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF20 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M36 HS BK 36% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 36% Filler by Weight and Mineral Filler, 36% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF30 IM2 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: UV Stabilizer, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Good UV.. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 6.89 GPa | 999 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-40FG-0700 40% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | Tangent; ASTM D790 |
Applied Composites 8072 Polyester SMC Industry Application: TransportationProduct Application: AutomotiveDistinct Features: Zero Shrink, Superior Class A Finish, Improved Impact, Accepts Mold CoatingInformation provided by Applied Compo.. |
|||
Flexural Modulus | 6.89 - 8.27 GPa | 1000 - 1200 ksi | |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |
|||
Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
PolyOne Edgetek® AT-30GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |