Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.95 GPa | 1010 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEP32 PC LNP* STAT-KON* DEP32 is a compound based on Polycarbonate containing 10% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Modulus | 6.95 GPa | 1010 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East) VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |