Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.33 GPa @Temperature 23.0 °C |
628 ksi @Temperature 73.4 °F |
EN ISO 178 |
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |