Polymer Property : Flexural Modulus = 66.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.460 GPa
66.7 ksi
ASTM D790
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium
Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne..