Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.655 GPa | 675.2 ksi | ASTM D790 |
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Flexural Modulus | 4.655 GPa | 675.2 ksi | ASTM D790 |
Lucent Polymers GPP-130 Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Chemically Coupled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |