Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.35 GPa | 1070 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | ASTM D790 |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN133G33SIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID LW4403A(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | ASTM D790 |
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by .. |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LS-3302 PC, 30% Glass Filled High Impact High-impact resistant PC/GF with 30% GF reinforcement for camera body tubeInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® LS-3302 PC, 30% Glass Filled High Impact High-impact resistant PC/GF with 30% GF reinforcement for camera body tubeInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | ASTM D790 |
Samyang Tribit® 1551GN30 PBT, Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN30 is an impact grade.Information pro.. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | ASTM D790 |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | ASTM D790 |
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 7.35 GPa | 1070 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HM-3301GL PC, Glass Filled High Impact PC/GF material that is used for electric and electronic partsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 7.35 GPa @Thickness 3.20 mm |
1070 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID LW4009A(W) PA6+GF/MF40%, Low Warpage Feature: Injection Molding, PA6+GF/MF40%, Low WarpageApplication: Automotive (Timing Belt Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |