Mechanical Properties Metric English Comments
Flexural Modulus 0.0539 GPa

@Thickness 6.40 mm
7.82 ksi

@Thickness 0.252 in
15mm/min; ASTM D790
LG Chemical KEYFLEX BT 3140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical
Flexural Modulus 0.0539 GPa
7.82 ksi
ASTM D790
SK Chemicals SKYPEL P137DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..