Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.87 GPa | 1140 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Flexural Modulus | 7.87 GPa | 1140 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Flexural Modulus | 7.87 GPa | 1140 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |