Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.90 - 17.9 GPa | 710 - 2600 ksi | Average value: 10.6 GPa Grade Count:42 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Flexural Modulus | 4.90 GPa | 710 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 GF13 ML2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
Flexural Modulus | 4.90 GPa | 710 ksi | ASTM D790 |
Ensinger Tecatron® XP-65 Compression Molded PPS Compound, 30% Fiberglass with 15% PTFE Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |