Polymer Property : Flexural Modulus = 727 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.01 GPa
727 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Flexural Modulus 5.01 GPa
727 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66
LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant.
Flexural Modulus 5.01 GPa
727 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP 9X07435
LNP* THERMOCOMP* is a compound based on Miscellaneous resin containing Proprietary Filler(s). Added feature of this grade is: Plateable.
Flexural Modulus 5.01 GPa
727 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific)
This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region.