Polymer Property : Flexural Modulus = 74.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.515 GPa

@Temperature 23.0 °C
74.7 ksi

@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET  (Unverified Data**)
Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont
Flexural Modulus 0.515 GPa
74.7 ksi
ISO 178
DuPont Performance Polymers Hytrel® 7246HS BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers