Polymer Property : Flexural Modulus = 773 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.33 GPa
773 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES
LNP* THERMOCOMP* JF003E is a compound based on Polyethersulfone resin containing 15% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 5.33 GPa
773 ksi
ISO 178
Polyplastics Duranex® 3105 Polybutylene Terephthalate (PBT), Standard, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 5.33 GPa
773 ksi
ISO 178
Polyplastics Duranex® 313RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 5.33 GPa
773 ksi
ISO 178
Polyplastics Duranex® 3105A Polybutylene Terephthalate (PBT), Epoxy adhesion improved, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..