Mechanical Properties Metric English Comments
Flexural Modulus 0.539 - 0.655 GPa
78.2 - 95.0 ksi
Average value: 0.596 GPa Grade Count:10
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu..
Flexural Modulus 0.539 GPa
78.2 ksi
ASTM D790
SK Chemicals SKYPEL G172D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-101 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-120 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-130 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-21 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion ..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-30 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-40 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-20 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,..
Flexural Modulus 0.539 - 0.637 GPa
78.2 - 92.4 ksi
ASTM D790
Daikin NEOFLON NP-3000 FEP Pellets
NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi..