Mechanical Properties Metric English Comments
Flexural Modulus 8.08 GPa
1170 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific)
LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System.
Flexural Modulus 8.08 GPa
1170 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12
LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System.