Polymer Property : Flexural Modulus = 8.4366 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 8.4366 GPa
1223.6 ksi
ASTM D790
E-Polymers TEKALOY® F50G30 30% Glass Fiber Reinforced PBT/PET Alloy
PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan..