Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.68 GPa | 1260 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC (Asia Pacific) LNP* LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 8.68 GPa | 1260 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF006I PA 66 LNP* THERMOTUF* RF006I is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 8.68 GPa | 1260 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Modulus | 8.68 GPa | 1260 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 8.68 GPa | 1260 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermotuf RF006I PA 66 LNP* Thermotuf* RF006I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region... |
|||
Flexural Modulus | 8.68 GPa | 1260 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA 30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 8.68 GPa | 1260 ksi | ISO 178 |
Polyplastics Duranex® 751SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 8.68 GPa | 1260 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |