Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.558 GPa | 80.9 ksi | ASTM D790 |
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: High Flow, Good StiffnessUses: Food containers, Small pails, Nursery containers |