Polymer Property : Flexural Modulus = 812.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.599 GPa
812.1 ksi
ASTM D790
Aclo Accutech ABS ABS833G20L Glass Reinforced
Flexural Modulus 5.599 GPa
812.1 ksi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0334M40CL Mica Reinforced Coupled
Flexural Modulus 5.599 GPa
812.1 ksi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0339G30CL Glass Reinforced Coupled