Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Asia Pacific) |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Europe-Africa-Middle East) CYCOLOY MC5220 is a 20% glass reinforced PC+ABS blend for injection moulding purposes. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
SABIC Innovative Plastics Lexan® LF1520 PC (Asia Pacific) |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Flexural Modulus | 5.88 GPa @Thickness 3.20 mm |
853 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUMID LW4303B(W) PA66+MF30%, Low Warpage Feature: Injection Molding, PA66+MF30%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
LG Chemical LUPOS GP-2205NB General Purpose SAN, 20% Glass Fiber Reinforced, Dimensional Stability, Anti-Bacteria LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 5 mm/min; ISO 178 |
Gromax BFM30-EL03N1 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 5.88 GPa @Thickness 3.20 mm |
853 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Flexural Modulus | 5.88 GPa @Thickness 3.20 mm |
853 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D 790 |
SABIC Innovative Plastics Ultem JD7902 PEI (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | |
Shinil Chemical SHINNANO PA-6 Polymer Nanocomposite Engine Cover and Bumper SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HT-8200G MPPE/PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VG-4920 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-8200G MPPE, 20% Glass Filled Material with good dimensional stability and 20% GF that can be used in pumps and impeller housingsInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® HT-8200G MPPE/PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VG-4920 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 30G3F Polybutylene terephthalate, 15% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60G3F Nylon 66, 15% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) ST60G6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | ASTM D 790 |
SABIC Innovative Plastics Valox® VGF4715 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.88 GPa | 853 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN135G33HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubric.. |
|||
Flexural Modulus | 5.88 GPa @Thickness 3.20 mm |
853 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |