Flexural Modulus 2.34 - 5.88 GPa
340 - 853 ksi
Average value: 3.72 GPa Grade Count:59
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..