Mechanical Properties Metric English Comments
Flexural Modulus 6.02 GPa
873 ksi
ASTM D790
Omni Plastics OmniTech™ ABS GR20 UV FD BK118, GY695 Flame Retardant
UL Approved MaterialOmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, ..
Flexural Modulus 6.02 GPa
873 ksi
ASTM D790
Omni Plastics OmniTech™ ABS GRC20 NA Glass Reinforced
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Flexural Modulus 6.02 GPa
873 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES
LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.