Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.610 GPa | 88.5 ksi | ASTM D790 |
NOVA Chemicals Novapol® TR-0535-U Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.610 GPa | 88.5 ksi | ASTM D760-66 |
Micropol Microlin ML20 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Flexural Modulus | 0.610 GPa | 88.5 ksi | ASTM D760-66 |
Micropol Microlin ML21 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Flexural Modulus | 0.610 GPa | 88.5 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a.. |
|||
Flexural Modulus | 0.610 GPa | 88.5 ksi | ASTM Test |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Flexural Modulus | 0.610 GPa | 88.5 ksi | ISO 178 |
LyondellBasell Hifax™ CA186 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent paintability and paint durability, good processabi.. |
|||
Flexural Modulus | 0.610 GPa | 88.5 ksi | ASTM D790 |
NOVA Chemicals Novapol® TR-0535-UG Hexene MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |