Mechanical Properties Metric English Comments
Flexural Modulus 9.05 GPa
1310 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66
LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding.
Flexural Modulus 9.05 GPa
1310 ksi
ASTM Test
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET
Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in..