Mechanical Properties Metric English Comments
Flexural Modulus 0.0650 GPa
9.43 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR107-93A Seal Grade TPU
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..