Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.53 GPa | 1380 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 9.53 GPa | 1380 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 9.53 GPa | 1380 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific) LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 9.53 GPa | 1380 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 (Asia Pacific) LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Flexural Modulus | 9.53 GPa | 1380 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON PX06418 PA 6 LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural. |