Polymer Property : Flexural Modulus = 9.535 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 9.535 GPa
1383 ksi
1.3 mm/min; ASTM D790
Ovation Polymers Nemcon™ E ABS 20CF
Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E ABS 20CF is a high modulus carbon fiber-rei..