Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.92 GPa | 1440 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant. |
|||
Flexural Modulus | 9.92 GPa | 1440 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific) LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 9.92 GPa | 1440 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing. |