Mechanical Properties Metric English Comments
Flexural Modulus 6.2485 GPa
906.28 ksi
UNI EN ISO 14125: 2000
CRP Technology Windform® XT Polyamide-Carbon Composite
WindForm™ XT Composite is a new generation material, in which the mechanical characteristics are excellent for Rapid Manufacturing. Black coloured compound polyamide and carbon based material with ..