Mechanical Properties Metric English Comments
Flexural Modulus 6.274 GPa
910.0 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK
LNP* THERMOCOMP* LF003 is a compound based on Polyetheretherketone resin containing 15% Glass Fiber.
Flexural Modulus 6.274 GPa
910.0 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific)
LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber.