Polymer Property : Flexural Modulus = 913.7 ksi
Polymer Property :
Flexural Modulus =
913.7 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
6.300
GPa
913.7
ksi
Secant; ASTM D790
Fiberfil® M-2501 BK Nylon 66, 40% mineral Filled, post industrial
Information provided by FIBERFIL Engineered Plastics