Polymer Property : Flexural Modulus = 922 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.36 GPa
922 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WF0039U PBT
LNP* THERMOCOMP* WF0039U is a compound based on PBT resin containing 15% Glass Fiber. Added features of this grade include: Flame Retardant and UV Stabilized.