Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.4088 GPa | 929.52 ksi | ASTM D790 |
Ecomass® 1080TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |