Mechanical Properties Metric English Comments
Flexural Modulus 6.56 GPa
951 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC
LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features include: Exceptional Processing, Non-Brominated & Non-Chlorinated Flame Retardant.
Flexural Modulus 6.56 GPa
951 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC (Asia Pacific)
LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing, Flame Retardant, Non-Br..
Flexural Modulus 6.56 GPa
951 ksi
ISO 178
Polyplastics Duranex® CRN7830 Polybutylene Terephthalate (PBT), Lower noise, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Flexural Modulus 6.56 GPa
951 ksi
ASTM Test
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..
Flexural Modulus 6.56 GPa
951 ksi
ASTM Data
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is ..