Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.66 GPa | 966 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RE004MPC PA 66 LNP* STAT-KON* RE004MPC is a compound based on Nylon 66 resin containing 20% Milled Carbon Fiber. Added features of this material are: Exceptional Processing, Clean Compound System, Electrically C.. |
|||
Flexural Modulus | 6.66 GPa | 966 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 6.66 GPa | 966 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber. |