Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.86 GPa | 995 ksi | ASTM D790 |
Nylene® PA6/6 Glass/Mineral Filled 7215 HS Nylon 6/6 15% Glass Reinforced/25% Mineral Filled.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 6.86 GPa | 995 ksi | ASTM D790 |
SABIC Innovative Plastics Lexan® LGK4010 PC (Asia Pacific) |
|||
Flexural Modulus | 6.86 GPa | 995 ksi | ASTM D790 |
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |