Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 1.6 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.7 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 4.8 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate, aged 3 hours at 816°C Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 3.2 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Charpy Impact, Unnotched | 171 J @Temperature 816 °C |
126 ft-lb @Temperature 1500 °F |
Longitudinal |
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate, aged 3 hours at 816°C Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |