Polymer Property : Charpy Impact, Unnotched = 17.6 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 17.6 J
13.0 ft-lb
Pacific Sintered Materials FX-227-T Infiltrated Steel Powdered Metal
Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1005-50All information provided by Pacific Sintered Metals.
Charpy Impact, Unnotched 17.6 J
13.0 ft-lb
PSM Industries Pacific Sintered Metals Infiltrated Steel FX-227-T Powdered Metal
Machines and plates well, Good in hydraulic applications, Moderate tolerance control Equivalent MPIF Specifications: FX-1005-50Information Provided by Pacific Sintered Metals, a division of PSM Ind..