Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 230 J

@Treatment Temp. 450 °C
170 ft-lb

@Treatment Temp. 842 °F
Aged 2000 hrs at 450°C
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel
Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform ..