Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 29.8 J | 22.0 ft-lb | |
Pacific Sintered Materials FX-233-T(HT) Infiltrated Alloy Steel Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals. |
|||
Charpy Impact, Unnotched | 29.8 J | 22.0 ft-lb | |
PSM Industries Pacific Sintered Metals Infiltrated Alloy Steel FX-233-T(HT) Powdered Metal Excellent combination of strength and shock resistance, Good for use in cams, pawls, sprockets and wear plates, Moderate tolerance controlInformation Provided by Pacific Sintered Metals, a division .. |