Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 1.59 J | 1.17 ft-lb | Exxon Mobil Method |
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin
(discontinued **) Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Puncture Energy | 1.58 J | 1.17 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 1236.85 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Puncture Energy | 1.58 J | 1.17 ft-lb | ExxonMobil Method |
ExxonMobil LLDPE LL 1236.86 Linear Low Density Polyethylene Resin Product Description: LL 1236 Series resins are butane LLDPEs with increased stiffness and a high melt index. They can be used alone or as a component in packaging and industrial film, blown or cast... |
|||
Puncture Energy | 1.59 - 4.41 J | 1.17 - 3.25 ft-lb | Average value: 3.22 J Grade Count:15 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |